Line 10: Line 10:
*Silicone-modified alkyd - [https://www.rustoleum.com/~/media/DigitalEncyclopedia/Documents/RustoleumUSA/TDS/English/CBG/Specialty/SPC-09_Specialty_High_Heat_TDS.ashx]
*Silicone-modified alkyd - [https://www.rustoleum.com/~/media/DigitalEncyclopedia/Documents/RustoleumUSA/TDS/English/CBG/Specialty/SPC-09_Specialty_High_Heat_TDS.ashx]
*Powder coating - not. 150C melting. [https://en.wikipedia.org/wiki/Powder_coating]
*Powder coating - not. 150C melting. [https://en.wikipedia.org/wiki/Powder_coating]
=Medium Temp=
*Galvanized pipe is recommended only up to 200C - [https://www.google.com/search?q=max+temp+of+galvanized+water+pipe&oq=max+temp+of+galvanized+water+pipe&aqs=chrome..69i57.10613j0j4&client=ubuntu&sourceid=chrome&ie=UTF-8]

Latest revision as of 20:48, 9 April 2020

  • Porcelain enamel - [1]
  • Aluminum is an option - [2]
  • Barbecue paint- maybe?

High Temperature Coatings

  • silicone modified alkyd resin - [3]. This is barbecue paint
  • Ceramic coating - [4]
  • Coating for power plant boilers - [5]
  • Interior of boilers - Apexior 1 - [6]. Sourcing - [7]
  • Silicone-modified alkyd - [8]
  • Powder coating - not. 150C melting. [9]

Medium Temp

  • Galvanized pipe is recommended only up to 200C - [10]