Hot Dip Galvanizing

From Open Source Ecology
Revision as of 17:05, 27 August 2020 by Marcin (talk | contribs)
Jump to navigation Jump to search
  1. Sand blast
  2. Base bath - 10 minutes min
  3. Base bath - 7 minutes min
  4. Flux - ammonium
  5. Actual dip - 3.5 minutes (until base metal reaches melt temp of 835F)
  6. Water - trapped water explodes, and is dangerous, so first dip is dangerous and venting must be assured.
  7. Zinc - 2400 lb blocks are the feedstock for hot dip baths.

https://www.aisc.org/globalassets/modern-steel/archives/2014/08/2014v08_galvanizing.pdf