Ethanol dehydration catalyst materials

Necessary equipment: 1. Laboratory scale 2. Three neck round bottom flask 3. Magnetic stirrer 4. pH meter 5. Centrifuge 6. High heat oven for calcination 7. Size 30-50 mesh

Reagents: 1. Al2O3 (gamma aluminium trioxide) BET SSA 200 m2/g 2. Na2CO3 3. Ti(SO4)2